== Parameters == ~- ||Beam radius || 3.5 cm || ||Suspension length || 40 cm || ||Diameter of suspension fiber (silica) || 550um (30kg) / 300um (10.8kg) || ||Number of suspension fiber || 4 || ||Mechanical loss of fiber || 6e-7 at 100Hz, 7e-8 at 1kHz || ||Mechanical loss of a mirror || 1e-8 || ||Number of coating layers (ITM) || 9 + cap || ||Number of coating layers (ETM) || 18 + cap || ||Mechanical loss of Silica coatings || 5e-5 || ||Mechanical loss of Tantala coatings || 2e-4 || -~ == Material properties == ~- ||Density of Silica || 2200 ||kg/m^3 || ||Young's modulus of Silica || 7.2e10 ||Pa || ||Poisson ratio of Silica || 0.17 || || ||Refraction index of Silica || 1.45 || || ||Thermal expansion of Silica || 5.1e-7 ||1/K || ||Specific heat per volume of Silica || 1.64e6 ||J/K/m^3 || ||Thermal conductivity of Silica || 1.38 ||W/m/K || ||dn/dT of Silica || 8e-6 ||1/K || ||Young's modulus of Tantala || 1.4e11 ||Pa || ||Poisson ratio of Tantala || 0.23 || || ||Refraction index of Tantala || 2.06 || || ||Thermal expansion of Tantala || 3.6e-7 ||1/K || ||Specific heat per volume of Tantala || 2.1e6 ||J/K/m^3 || ||Thermal conductivity of Tantala || 33 ||W/m/K || ||dn/dT of Tantala || 14e-6 ||1/K || -~